UralInduktor · metallurgical equipment manufacturing and supply
We will call back within 10 minutes

Materials for induction melting

Fitting mixes for induction furnaces

Alloy selection and melting mode Step-by-step stuffing Sintering and wear control

UralInduktor selects and supplies lining mixtures from partners for induction melting furnaces. When selecting, we take into account the metal brand, the composition of the slag, temperature, the design of the furnace and the work schedule. This makes it possible to compare materials according to the conditions of use and the cost of melting.

Below is a guide for technologists, foundries and supplies: what mixtures are used, what to check before filling, how to estimate the consumption and what data to prepare for the application. The main area of consideration is needle induction furnaces without a core with a printed working lining. For channel furnaces, replaceable crucibles and special vacuum processes, a separate selection is required.

What is Lining Induction Furnace

Lining is a system of refractory and protective materials inside the furnace. The working layer holds the melt, perceives the action of metal and slag, heating, cooling and mechanical loads during loading. Its condition affects the safety of melting, the purity of the metal, the useful capacity and the stability of the equipment.

Lining is formed from the mixture directly in the furnace. The mixture is compacted according to the adopted technology, and the necessary structure is obtained at the first warming up and sintering. Replacement finished crucible is another constructive solution: instructions for its installation can not be automatically transferred to the printed crucible.

Induction furnace wall circuit from melt through working lining and protective layers to inductor
Conditional arrangement of materials in the wall of the furnace. The composition, order and thickness of the layers are determined by the project.
Materials for different areas of the furnace
ZoneTaskWhat is selected
Bottom and Work WallMetal contact, wear and thermal cyclesBasic printed mixture agreed with metal and slag
Upper belt and collarShocks furnace charge, contact with slag, work outside the hottest zoneCompatible mass for upper belt with suitable type of ligament
Plum SockDirectional metal flow and local wearMass, plastic material or shaped element for sock
Inductor SprayingSurface protection and alignment on the side of the coilSpecial coating with project properties
Separation layerPossibility of lining movements during heating and coolingMica or other project material
Repair sitesRecovery of acceptable local defectsCompatible repair structure with separate instructions

One mixture should not automatically replace all the listed materials. For example, the dry working mixture and the collar material may have different ligaments and different hardening conditions. Additional insulating layers can also not be introduced arbitrarily: they change the temperature field and the geometry of the furnace.

Inductor Spray and Collar

The coating is applied to the inner surface of the inductor as a separate protective layer. Working printed liner is formed from the side of the future melt, with the intermediate layers provided by the project. The collar is located at the top of the furnace; material is selected for it, taking into account the shocks of the furnace charge, contact with the slag and the temperature of this zone.

Types of lining mixtures

In foundry practice, mixtures are often separated by chemical basis. This classification helps to narrow the choice, but does not replace the passport of a particular material. In one group there are compositions with different granularity, ligament, expansion and sintering mode.

Comparison of the main families of mixtures
FamilyWhere to ConsiderKey limitation
Acid quartz based on SiO₂Many iron smelting processes; separate coordinated processes with copper alloys or steelCompatibility with main slags and active melt components; sensitivity to selected thermal conditions
High-fat and aluminosilicateVarious black and colored alloys - depending on the composition and ligamentsAl₂O₃ does not in itself determine suitability; wetting, phase composition and ligament temperature are important
Spinels and spinel-formingMany steel smelting processes; individual modes of smelting cast iron and other alloysIt is necessary to agree on the expansion under heating and the mode of formation of the working structure
Basic, based on MgOProcesses where resistance to main slag and related metallurgy is requiredMoisture sensitivity of some components, thermocycles and sintering features
Special formulations for non-ferrous metalsAluminum and copper alloys taking into account fluxes and temperatureProperties are required for this melt; non-wetting additives or SiC components are possible

The term "neutral" is commonly used for a number of high-glycose and spinel systems. It does not mean chemical inertness to any melt. A material with a higher passport temperature is also not necessarily the best: at too low a temperature of a particular process, its ligament may not form properly.

Dry lining mixture in a metal tray next to the scoop and neutral packaging
Visualization of dry refractory mixture. The color and size of the grains do not allow you to determine its brand or suitability.
What to read in the passport mixture
IndicatorWhy is it necessary to select
Application and chemical compositionCheck compatibility with metal, slag and fluxes
Working and short-term allowable temperatureSeparate the standard mode and time-limited excess; not to be confused with fire resistance
Grain composition and method of layingChoose the appropriate sealing method and snap-in
Density after sealingCalculate the mass of the material in the project volume
Type of ligament and program of first heatingUnderstand how the material gains strength and what equipment is allowed
Change in size when heatedCheck the consistency of the material with the lining design
Shelf life, storage and security passportOrganize acceptance, warehousing and dust handling

How to choose a mixture for metal and melting mode

Selection begins with the actual process: a list of metal grades, maximum temperature, exposure time and slag composition. Especially important are transitions between alloys, modification in the furnace, the use of fluxes and work with contaminated furnace charge. The names “cast iron furnace” or “aluminium furnace” are not enough for the final choice.

Examples of alloys and preliminary directions of selection
Group and examples of stampsWhat systems are considered firstWhat determines the final choice
Grey cast iron: SCH15, SCH20, SCH25, SCH30Often quartz; under special requirements - agreed aluminosilicate or high-glynozemyActual chemical composition, overheating, exposure, slag, furnace charge condition and number of cold starts
High strength cast iron: HF40, HF50, HF60Quartz or qualified mullite-forming and high-clay-earth systemsWhere modification is performed, contact with magnesium-containing residues, temperature and nature of wear of the lower part of the crucible
Carbon Cast Steel: 20L, 35L, 45LOften high-clay spinel-forming systemsDeoxidation, composition and basicity of slag, release temperature, exposure time and melting schedule
Low alloy cast steel: 20GL, 35HGSL, 40HLHigh-clay or spinel-forming systems, confirmed for the wholeContent of manganese, chromium and other active elements, metallurgical additives and slag
High manganese steel: 110G13LBasic magnesia or specially confirmed neutral systemsBasic slag, oxidation mode, exposure time and metal contamination requirements
Corrosion-resistant cast steel: for example, 12Х18Н9ТЛHigh-purity high-clay or spinel-forming systemsFull chemical composition, deoxidation, temperature, slag and allowable inclusions from lining
Copper: M1, M2Compatible mullite-forming or high-clay-earth systems; individual quartz solutions - only after confirmationOxidative mode, exposure time, metal purity and first heating program
Brass: L63, LC59-1Specialized systems for copper alloys, including individual mullite or SiC formulationsLoss of zinc, fluxes, slag, alloy change and melt interaction with lining
Bronze: BRO 10 F 1 , BRO 5 T5 C 5Compatible systems for copper and bronze, confirmed for a specific brandTin, lead and other components, fluxes, oxidation and purity requirements
Foundry aluminum alloys: AK7h, AK9h, AK12Special high clay or mullite-forming materials with reduced wetting aluminumFlues, magnesium in alloy, exposure temperature, metal penetration and ligament formation temperature
Nickel heat-resistant and other reactive alloysHigh-purity lining, consistent with technology; vacuum smelting is considered a separate projectAlloy chemistry, atmosphere or vacuum, allowable pollution and furnace design
Frequent change of different alloysA system whose applicability is confirmed for the entire list of floatsConsistency of grades, furnace cleaning, transition metal, mutual pollution and the most aggressive mode

The alloy brand in the table is a convenient starting point, but not a ready-made purpose of the material. Two melts of the same brand can differ in furnace charge, slag, acidification, temperature and aging. Before delivery, chemical analysis or process instructions are checked and the compatibility of a particular mixture with all operations in the furnace.

Slag and fluxes

Evaluate their composition and quantity, time of contact with the wall, metal drift and removal practice. Conditional division of slags into acidic and basic is useful, but one basic factor for choice is not enough: other oxides, fluxes and temperature are also important.

Office hours

Constant hot conditions and daily stops create different loads. The duration of melt exposure, the number of cold starts, the frequency of alloy changes and the ability to perform the prescribed sintering program are taken into account.

Furnace construction

Required capacity, power, frequency, working profile and design thickness lining. An arbitrary increase in thickness reduces the useful volume and changes the conditions of electromagnetic communication; a decrease reduces the margin to extreme wear. The geometry is consistent with the documentation for the furnace.

Trial campaign

After documentary approval, the new material is evaluated under comparable conditions. Record the mass of the stuffing, temperature curves, tons of molten metal, repairs and wear profile. A reasonable result requires a comparison of the same alloys and modes, not just the number of floats.

Where different types of lining are used

The term "lining induction furnace" combines different designs. The choice depends not only on the metal, but also on the type of furnace, heating method, maintainability and purpose of each site. The technology of dry filling of crucible furnace can not be transferred without verification to the inductor channel, dosing furnace or finished crucible.

Lining application by type of equipment
Equipment or areaTypical direction of decisionWhat should not be transferred automatically
Tigel induction furnace without coreMonolithic dry stuffed working lining; separate materials for bottom, wall, top belt, sock and inductor coatingMixture composition, thickness, sealing method and first start mode from another furnace
Channel Induction FurnaceSeparately design bath, canal and inductor connections; printed, concrete and shaped solutions are possibleTechnology of crucible furnace wall on narrow channels and couplings
Exposure, Dosage or Low Pressure Furnace for AluminumHigh clay and other aluminum-compatible materials with wetting control; monolithic and prefabricated elements are usedHigh Temperature Steel Oven Program and Universal Mixture for All Zones
Furnace with replaceable ready-made crucibleReady-made crucible, support and back-up system for equipment documentationRules for layer-by-layer stuffing of a monolithic working wall
Vacuum induction melting and reactive alloysHigh-purity system selected by allowable inclusions, atmosphere, vacuum and bottling methodNormal selection only at the maximum temperature
Top belt, drain sock and local repairCompatible special masses, plastic materials, coatings or shaped elements for the purpose of the zoneThe main dry mixture without checking the ligament, adhesion and thermal mode

For purchase, it is useful to draw up a statement by zones: main working mixture, upper belt and sock, inductor coating, separation layer, repair material and tooling. This reduces the risk that a suitable mixture will be applied to the wrong node.

Lining Induction Furnace

The task of stuffing is to get the provided density and a uniform wall without voids, impurities and pattern displacement. The repeatability of the process depends on the condition of the furnace, the preparation of the tooling and the chosen sealing method. The finished mixture is used in the form indicated in its technical documentation.

Methods of working lining
MethodFeatureWhat they control
Layer seal by hand tool or portable machineThe material is laid and processed according to the adopted technological mapMass of portions, processing of transitions, tool access and density uniformity
Vibration Seal Through TemplateFluctuations are transmitted mixtures from special equipmentRigidity and pattern centering, vibration mode and signs of mixture stratification
Wet ramming mass or refractory concreteIndependent technology for materials intended for itLiquid dosing, styling, hardening, drying and first heating
Installation of the finished crucibleThe working vessel is made in advanceResistance, gaps, filling and warming up according to the documentation for crucible and furnace

The dry mixture should not be turned into wet by adding water. The vibration method also does not mean that any material can be compacted longer or stronger: the parameters are chosen for a particular mixture and equipment. When switching to another method of stuffing, the technological map is revised.

Pneumatic double impact blower, air distributor and chain suspension
Pneumatic vibrator with two impact heads for sealing through a steel pattern. Image by photo; installation in the oven is not shown.

Manual Electric Vibrator For Lining

Manual electric vibrator is used to seal the dry stuffing mixture when lining a crucible induction furnace. The electric drive creates vibrations that are transmitted to the material through the installed snap-in. Handles allow the operator to guide the tool through the work area.

The image shows a vibroblock, a bottom plate and replaceable nozzles of different shapes. The type and dimensions of the nozzles, the sequence of their application and the sealing mode are selected according to the technological map for the specific mixture and geometry of the lining.

Manual electric vibrator with handles, bottom plate, flat, combed and profile nozzles
Manual electric vibrator with replaceable nozzles. Image from the photo of the provided sample.
What to check when selecting a hand-held vibrator
ParameterWhat to Agree
Bottom of the crucibleSize and shape of the bottom plate, access to the transition between the bottom and the wall
Wall and annular gapProfile and width of the nozzle, the possibility of processing by circumference and height
Nozzles and extension cordsComposition of the kit, length of the working part, fastening and compatibility with the vibroblock
Mixture and method of fillingSuitability of the material for the selected tool, portions of the mixture and the order of sealing
Power supplyVoltage, number of phases, network frequency and specific passport connection
Operating modePower and weight of the machine, frequency and force of oscillations, allowable duration of work

Manual machine requires consistent processing of the entire working area. The technological map records the passages and seal control; selection only in terms of engine power or furnace capacity does not determine the appropriate filling mode.

Control before filling
Object of verificationWhat needs to be confirmedWhy it matters
Furnace and workplaceThe oven is empty, brought to a safe state; work is allowed according to the accepted procedureEliminate the effects of melt, energy and moving nodes
Previous liningReason for replacement and actual wear profile recordedDo not repeat the hidden cause of destruction
Inductor and its shadingNo damage detected; surface and drying conform to documentationSave coil protection and design geometry
Cooling and protective devicesChecks performed in the prescribed mannerPrevent launch with inoperable protection or cooling defects
MixtureTrue brand and batch; packing is complete; shelf life and storage conditions are metDo not use undercooked, contaminated or unconfirmed material
Template and ToolDimensions, centering, rigidity, cleanliness and sealing method are consistentGet a uniform wall and avoid inclusions

Phased sequence of work

Below is the framework of the technological map for crucible furnace with monolithic dry lining. Specific portion masses, layer height, tool, vibration mode, thickness and heat schedule are entered only from the documentation on the selected mixture and furnace.

Step by step stuffing working lining
StageWhat they doControl Record
1. Approval of a taskFixed furnace, working profile, list of alloys, slag and fluxes, selected materials by zones, sealing method and first start programNumber of technological card, drawing, passport mix and responsible persons
2. Safe preparationThe furnace is stopped, cooled and isolated according to the rules of the enterprise; they issue a permit, organize dust removal and waste collectionAdmission to work, verification of the absence of dangerous energy, protection measures applied
3. Dismantling and wear mapThe old lining is removed without damaging the stored items. Before stripping, the wear profile is photographed and measuredReason for replacement, photos, thickness at control points and defects detected
4. Inspection of designCheck the inductor, its insulation and coating, supports, upper and lower elements, cooling, grounding and the provided protection against metal penetrationThe act of inspection and the list of eliminated comments
5. Surface preparationRestore and level the inductor smear. All elements that are supposed to be dried are dried according to their own instructions.The result of the inspection, confirmation of the dry state and project geometry
6. Protective and Separative LayersInstall mica or other separation layer, leakage control grid and other elements of the project without breaks and random adhesive additivesMaterial, pattern of overlaps and connections, no damage
7. Input control of the mixtureVerify the purpose, batch, period, integrity of packaging and storage. Moisturized, contaminated or mixed with residues mass is separated until the decision of the specialistNumber of lot, number of bags and weight, packing condition, material temperature if necessary
8. Check templateThe template is cleaned and checked by diameter, conicality, height, roundness and stiffness. Provide a method of fixation and the option of removal or meltingActual dimensions, deviations, control risks and how to work with the template
9. Formation of bottomThe mixture is served in measured portions and compacted with the accepted method. Form the design level, thickness and transition to the wall without loose anglesWeight of the mixture at the bottom, high-altitude marks, tool and parameters from the approved map
10. Template CenteringThe template is installed on the prepared bottom, fix and measure the annular gap in several directions and in heightGaps, verticality, elevation and signature of the receiver
11. Filling the wallThe ring space is filled in a given sequence. Each portion is distributed evenly, without polluting the mixture and without changing the patternMass of each portion, level of filling and time of operation
12. Wall SealThey work only by a coordinated method: a hand or pneumatic instrument, a submersible vibrator or vibration through a template. Methods are not arbitrarily combinedTool type, specified mode, actual time, operator and comments
13. Upper transition and drainForm the upper belt, collar and drain sock from compatible materials in the sequence adopted for this designMaterial of each zone, joint preparation, mass and geometry
14. Final acceptance of stuffingCheck the total consumption with the calculation, profile, pattern position, top mark, lack of extraneous inclusions and completeness of all zonesMass balance, control dimensions, photo fixation and heating resolution
15. First warming and sinteringPlace measurement tools and execute an approved program. Record the actual temperature and time at each stage, deviations and actions of the responsible personPlan and actual curve, measurement locations, decision to switch to smelting
16. The first working swimLoad the furnace charge in the prescribed way, without damaging the new wall. Fixed alloy, temperature, exposure time, slag and post-launch observationsThe passport of the first swimwear, comments and the decision to start a working campaign
Control points without moving to the next stage
Point of acceptanceWhat needs to be confirmedWho records
After Inductor InspectionComments removed, shading and retained items ready to closeResponsible for the furnace and electrical part in the order of the enterprise
After installation of protective layersThe system is assembled according to the project, the separation layer and leakage control are not damagedResponsible for lining work
After the bottom deviceThickness, level, transition profile, mass and seal are acceptedMaster or Technologist
After Centering TemplateThe clearance and position are within the tolerance of the approved drawingMaster or Technologist
Before the first heatingAll zones completed, flow and geometry recorded, temperature measurement preparedCommission or designated persons responsible
After the sintering programActual curve checked, deviations reviewed, further work allowedTechnologist and responsible for furnace operation

Work with dry refractories is organized with local dust removal and protective equipment for assessing working conditions and a safety passport. Suitable industrial dust removal is used for cleaning; dry sweeping and blowing with compressed air spread dust. The dust formation during the dismantling of the old lining also requires control.

In order not to restore the installation history from memory, use the form to be filled out from the package. It links the batch of material, geometry, mass by stages, parameters from the approved map and the actual curve of the first start.

Typical mistakes when filling lining

Most defects cannot be reliably determined only on the outer surface of the finished wall. Therefore, error prevention and recording of actual parameters is more important than trying to fix an already closed layer.

Errors, consequences and prevention measures
ErrorPossible consequenceHow to warn
Use of wet or contaminated dry mixtureUneven sealing, gas formation, ligament defects and unpredictable first heatingClosed dry storage, batch inlet control and insulation of damaged packaging
Unauthorized addition of water, ligaments or other mixtureChange in composition, sintering, volume and chemical resistanceApply the finished material without changes; any mixing is made out as a separately developed recipe
Irregular or undryed inductor coatingVariable wall thickness, local stresses and risk of defect in the protective systemCheck the profile and dry condition before installing closing layers
Breaks of the separation layer or damage to the leakage control systemViolation of the design protection system and the impossibility of correct diagnosisInstall according to the drawing, protect from the tool, take to the backfill
Insufficiently rigid, deformed or displaced patternDifferent wall thickness, change of working volume and local overheatingCheck the size and stiffness, fix the pattern, measure the gap in circumference and height
Random portion size and missing seal areasLoose zones, layering and local metal penetrationMeasure mass, keep a log of levels and work along the route specified in the technological map
Excessive or inconsistent vibrationBreakdown of the grain composition, displacement of the pattern or damage to the protective layerUse parameters and snap-in confirmed for the selected mixture and geometry
Arbitrary combination of manual stuffing and vibration through the templateDifferent density and boundaries between processing zonesChoose one agreed method or describe the transitions in the map in advance
Application of one mass for wall, collar, wear and repair without inspectionEarly destruction of the cold upper belt, joints or drain zoneSelect materials according to the function of each zone and check their compatibility
The first heating without temperature recording at specified pointsUnable to confirm the formation of the ligament and understand the defectPrepare the devices in advance and keep a plan-fact for each stage
Impact loading of heavy furnace charge on new wallChips and cracks until a stable working structure is formedFollow the loading instruction, size and order of laying furnace charge for the first smelting
Lack of mass balance and photo fixationHidden geometry deviation and data loss for campaign analysisCheck the calculated and actual flow rate, fix the control points before heating

Sintering and starting the furnace

The first warm-up forms the working structure of lining. For materials with water or liquid binder to the high temperature stage, the envisaged removal of moisture and products of the ligament is required. Dry mixes also have their own program of first heating: the lack of added water does not cancel the launch requirements.

For many dry padding systems, there is a sintered working layer, a transition area, and a less sintered or powdered area on the cold side. Therefore, sintering the entire thickness is not a universal goal. At the same time, the looseness on the surface in contact with the metal cannot be explained by the presence of a normal cold zone.

What should be specified in the program of the first start
ParameterWhat is fixed
Applicable materialMarku, batch, thickness and combination with materials of neighboring zones
TemplateMaterial and method of application: removable, melted or otherwise provided
Source and stage of heatingMethod of heating, permissible loading, sequence of stages
Temperature and exposureTemperature change rates, reference values and exposure duration
MeasurementsType and location of sensors, medium to be measured and record of actual curve
Cooling or switching to smeltingConditions for the completion of sintering, allowable stops and subsequent start

There is no universal program “so many degrees per hour for any furnace”. The mode depends on the composition, ligaments, thickness, heating method and template design. The temperature of the metal, the surface of the template and the depth layers of the lining differ: the readings of one device are interpreted taking into account the place of measurement.

The order of cooling and re-starting is also taken from the documentation for a particular system. For different linings, recommendations can differ significantly. You can not independently appoint accelerated cooling, pour lining with water or transfer the mode from another furnace just because its capacity is similar.

What affects the durability of lining

In operation, chemical wear from metal and slag simultaneously act, blurring the flow, blows furnace charge and thermal stresses. The resource depends on their combination. The more expensive mixture does not compensate for systematic overheating, violation of the padding or damaged inductor protection.

  • Maintain a consistent release temperature and exposure time; record deviations.
  • Control the condition of the furnace charge and its loading according to the instructions of the furnace. Wet furnace charge, closed containers and the formation of a hanging vault require the necessary preventive measures.
  • Remove the slag and thicken the allowed way without damaging the working wall.
  • Record cold launches, alloy changes, repairs and non-standard events.
  • Control the thickness and condition of the lining according to the established schedule and at the same control points.
Signs of wear and direction of inspection
MonitoringPossible causesWhat is being checked
Accelerated wear at the metal mirrorSlag, fluxes, long exposure at one levelSlag chemistry, temperature log and local thickness
Local production at the bottom of the wallMelt fluxes, chemical effects, geometry and non-homogeneous fillingWear profile, smelting mode and installation map
Cracks or chips after stoppingThermocycles, mechanical loads, structural featuresCooling and starting conditions, defect depth and residual thickness
AbundantlyComposition of slag and furnace charge, temperature, surface wettingCause of deposits and acceptable method of cleaning
Loose working surface after the first warm-upInappropriate mode, material or seal violationActual temperature curve, batch and filling technology
Metal inclusions or signs of penetrationCracks, lack of density, incompatibility or wearThe state of the entire protective system; admission to further work is taken by the responsible person
Protection signal, suspicion of water or metal leakagePotentially dangerous system damage or malfunctionOperate according to the emergency instructions of the furnace; bypassing or resetting the protection does not replace the diagnosis

This table helps to organize the diagnosis, but does not allow the continuation of melting when a dangerous sign is detected. In case of an emergency signal, the established procedure for stopping and handling the melt is performed. The order of operation of cooling and other systems determines the instructions for the equipment.

Metal leakage and penetration control complements the lining inspection. The absence of a signal does not confirm a sufficient residual thickness. The maximum thickness, acceptability of defects and conditions of decommissioning of the furnace are set in the documentation for a particular furnace and its lining.

Repair and replacement of lining

Local repairs are considered when the survey confirms the admissibility of restoration and the safety of the rest of the lining. It needs a compatible composition, suitable surface preparation and its own mode of hardening, drying or heating. Applying the mass on top of the hardened or damaged base does not eliminate the cause of wear.

Surface coating, repair weight and new working padding perform different tasks. The coating cannot restore the lost load-bearing thickness or hide a dangerous crack. In case of unacceptable wear, metal penetration or inability to confirm the suitability of the lining, the decision is made according to the procedure of decommissioning and replacement.

When replacing, it is useful to save photos and measurements in height and circumference of the crucible. The wear map shows where to look for the cause: in the selection of the composition, filling, loading, slag mode or heat cycles. Old recovered material is not returned to the new pad without specially developed and proven technology.

How to calculate the flow rate of the lining mixture

For the order, the volume of each zone is calculated and multiplied by the density of the corresponding material after compaction. The grain density and bulk density of loose powder for this task are unequal. The data is taken from the passport of the mixture or the agreed installation experience.

Mass of mixture volume of filling density after sealing

For a simplified cylindrical crucible with a solid flat bottom, the volume of working padding can be estimated as follows:

V = π / 4 × [(D² − d²) × H + D² × t]

Here, D is the outer diameter of the working filler; d is the inner diameter of crucible; H is the height of the wall from the upper surface of the working seabed; t is the thickness of the working seabed. All dimensions are set in metres, volume in m³. The height H does not include the thickness of the bottom, so it is not counted twice.

Educational example of calculation for cylindrical form
Source data or resultValue
Outer diameter of working pad D0,60 m
Inner diameter of crucible d0,50 m
Wall height H0,50 m
Bottom Thickness T0,08 m
Conditioned density after sealing2 200 kg/m³
Estimated wall and bottom volume0,0658 m³
Mass in project volumeAbout 145 kg
With conditional stock for installation 10%About 160 kg before rounding by packing

The dimensions, density and stock in the example are conditional: this is an explanation of the method, not the recommended lining design. For a real oven, taper, transitions, collar, sock and other zones are separately taken into account. The stock is agreed on the method of installation; the inductor coating and repair materials are considered separately.

How to compare the cost and resource of mixtures

The price per kilogram shows only the cost of purchase. For production comparison, you need the cost of one campaign and the tonnage of quality metal for this campaign. Campaign is the period of work from the installation of a new working lining to its replacement.

Lining cost, ₸/t = cost per campaign / tonnage per campaign

Comparison of the two options
IndicatorWhat to include or record
Materials per campaign, ₸The main mixture, materials of neighboring zones, repair and delivery
Installation and putting into operation, ₸Preparation, labor, equipment, energy for coordinated heating
Downtime, h and ₸Replacement, repair and start-up time; the cost of downtime is calculated according to the methodology adopted at the enterprise
Smelting for the campaign, tComparable tonnage according to the same quality criterion
Operating conditionsAlloys, temperatures, shutter speeds, cold starts and repairs
Profile of wear and reason for replacementMeasurements at control points and conclusion of the campaign

It is incorrect to compare only the number of floats if the mass of the garden, the temperature or the work schedule differ. Persistence in someone else's shop is useful as a guide for discussion, but is not a guarantee for another furnace. The expected result is specified according to the operation data and agreed tests.

Reception and storage of lining materials

When accepting check the brand, mass, batch numbers, date of manufacture, expiration date and a set of documents. Check the packaging and traces of moisture. Material with impaired storage conditions is separated from a suitable to the decision of the responsible specialist; drying on site does not mean automatic restoration of properties.

The mixtures are stored according to the requirements of delivery: in a suitable dry room, in a closed package, with protection against condensate and pollution. The parties are kept identifiable, the open bags are counted separately. You can not independently sift the finished composition, add a bunch or mix the remains of different brands for the sake of economy.

Frequently Asked Questions about Lining and Filling

Is it possible to pick up the mixture only by the capacity of the furnace

Oh, no. Capacity helps to estimate flow, but does not determine chemical compatibility. For selection you need alloy, temperature, slag, operating mode and working lining design.

Is it enough to know the brand of alloy

Oh, no. The brand specifies the composition range, but actual chemical analysis, furnace charge, slag, fluxes, deoxidation, temperature, and aging are important for selection. Examples of marks on the page show only the direction of the primary selection.

Which lining is better for cast iron

For many processes, the quartz system is suitable. Under aggressive conditions, a special cast iron composition or another task, alternatives are considered. The final choice is made according to the conditions of a particular melting.

Is one mixture suitable for steel and aluminum?

Only if its applicability to both processes is confirmed. There are chemical effects, temperature and conditions of formation of the ligament. Universality can not be determined by one value of fire resistance.

Is it necessary to add water to a dry filling mixture

Not if the documentation defines it as a finished dry mixture without the addition of liquid. Materials for wet stuffing and concrete are separate compositions with their own dosing and drying.

Is it possible to add boric acid or another ligament on your own?

Additives are not introduced into the finished mixture without an agreed recipe and instructions. The change in the ligament affects the sintering, properties, and operating range of the material.

What should be the thickness of lining

It is determined by the project of the furnace, taking into account the selected system. The initial profile, bottom, transitions and marginal wear are important. A table of power or capacity without a drawing does not replace this data.

How long does it take to sinter

The duration is specified by the program for a specific mixture and design. It is influenced by the ligament, thickness, pattern, heating and aging. There is no universal time per ton of capacity.

Is it possible to change the method of filling without changing the mixture

The ability to check the documentation of the material. For a new tool or vibration equipment, agree on the technological map and quality control of the installation.

Which is better manual stuffing or vibration through a template

The best method is confirmed for a specific mixture, the geometry of the furnace and the available tooling. Vibration through a rigid pattern can increase repeatability, but requires proper centering and a given mode. Unauthorized unification of methods creates unequal density.

Do I need a separate mass for the collar and drain sock?

Often yes, because the upper belt works at a different temperature, gets hit by a furnace charge and contacts the slag, and the sock experiences a directional flow. The possibility of using the main mixture in these zones should be directly confirmed.

Is the powder zone normal outside the baked layer

For a number of dry padding systems, such a zone is provided by the design. Its acceptability is assessed for a particular material. The loose working surface and through defects require separate inspection.

How to determine the end of the resource

Focus on the specified maximum thickness, working surface condition, inspection results and criteria of the furnace manufacturer. The number of floats by itself does not confirm the suitability.

Is it possible to increase the resource by coating

The coating can perform the surface function provided by the technology. It does not replace the main lining and does not restore the unacceptably worn wall.

What data is needed for an unknown brand of the old mixture

Send data to the furnace, metal grades, temperature, description of the mode, drawing or size of the crucible and photos of lining. The appearance of the powder can not be reliably determined brand.

Selection and supply of lining mixtures

UralInduktor will help you choose lining mixtures from partners under the conditions of your induction furnace. In the application, you can specify the need for basic stuffing, collar and sock materials, inductor smearing and repair compositions. The set of delivery, documentation, cost and time will be agreed for the chosen solution.

What data to send for selection
DataWhat to indicate in the application
EquipmentModel, capacity, power and operating frequency of the furnace
MetalBrands of alloys, composition of furnace charge, modification and deoxidization in the furnace
TemperatureNormal and maximum metal temperature, exposure time
Slag and fluxesMaterials used, dosages when available and method of disposal
Working hoursBoat in shift, duration of stops, cold starts and alloys change
GeometryDrawing or dimensions of working cavity, bottom and wall; template type
Current LiningFamous brand, mass of stuffing, campaign tonnage, photos and reason for replacement
InstallationAppliance used, method of stuffing and available heating program
ProcurementRequired volume, city of delivery and desired time

If some of the data is not yet available, start with a model of the furnace, metal grades, temperatures and photos. We will clarify the missing parameters for technical selection and delivery calculation.

Selection and estimate

Get an equipment selection or a project calculation — fill in the form

An engineer will contact you, clarify the task and suggest a solution for your production process.

  • Equipment selection for your metal, operating mode and output
  • Cost, lead time and delivery arrangements
  • Response within one working day

Equipment selection and estimate request

Technical specification or equipment passport PDF, DOC, XLS, JPG or PNG, up to 10 MB
In touch with you

Let's discuss your task

  • Main contact number+7 (775) 853-40-95Sales department and engineering centre
  • Emailstasgross.ru@gmail.comResponse during the working day
  • Main office addressAstana, Saryarka district, Radisson hotel, office 4
  • Office hoursMon–Fri, 9:00–18:00GMT+5 (Astana)
Comparison of proposals

We'll compare commercial proposals
and offer our own option.

Send us another company's proposal — we will compare the equipment list, configuration and cost.