Shot blasting machine for forgings
After forging and stamping, dense scale remains on the part. Shot blasting removes it before machining, inspection and heat treatment. The machine type is chosen by the forging mass and whether it is processed in batches or piece by piece.
Quick estimate and consultation
An engineer will select a machine for your parts and send a calculation.
Up to 300 kg — tumbling, up to 3,5 t — drum with belt, heavier — table or hanger.
Serial batches are more efficient to run as a load, single heavy items — piece by piece.
Blind cavities and pockets require rotating the part in the shot stream.
For machining, flaw detection or coating — the modes differ.
Which units are suitable
Forgings are strong and tolerate tumbling well, so in series production drum machines usually win:
| Forgings | Loading | Type of installation | Models |
|---|---|---|---|
| Small, in batches | up to 300 kg per cycle | Drum tumbling | УИД-3110, УИД-3113 |
| Medium, in batches | up to 1 500–3 500 kg | Drum with belt | УИД-15, УИД-28 |
| Flat and disc-shaped | up to 400–1 200 kg | With a rotating table | УИД-3512, 3515, 3518 |
| Large, piece by piece | Ø up to 1 200–1 500 mm | Crane-type | УИД-3710, УИД-3720 |
What to look at when choosing
- Scale density. Scale after forging adheres more firmly than rust: the mode and the shot fraction are selected for it, otherwise the cycle time grows.
- Part temperature. Forgings are fed for cleaning cooled — hot metal damages the belt, seals and shot.
- Load per cycle. For drum machines, the batch mass is calculated, not that of a single part: the size depends on it.
- What comes next in the route. Before flaw detection, cleanliness requirements are higher than before rough machining.
What to send for selection
The mass and dimensions of a typical forging, the batch mass, the production program, the surface condition and the next operation in the route. The engineer will select a size and prepare the proposal.
A summary table for all products — on the page of shot blasting machine selection.
Questions about selection
How does cleaning forgings differ from cleaning castings?
Forgings are stronger and tolerate tumbling in a drum calmly, and it is dense scale that has to be removed, not burn-on. That is why drum machines are chosen more often for forgings in series, and a table or hanger for castings.
Can hot forgings be loaded?
No. The part is fed cooled: hot metal damages the conveyor belt and the chamber seals and accelerates shot wear.
What is the productivity of drum machines?
It depends on the load mass, the number of turbines and the required degree of cleaning. Guidelines for each model — in the cards of the section drum machines.